| Sign In | Join Free | My benadorassociates.com |
|
Brand Name : MEILONG
Model Number : 3/8'' OD x 0.065'' WT
Certification : ISO9001:2015, PED 97/23/EC
Place of Origin : China
MOQ : 10000 feet
Payment Terms : L/C, T/T
Supply Ability : 150000 meters per month
Delivery Time : 10 days (for our required MOQ)
Packaging Details : Level wound coiled on wooden spool, and wooden case packing
Material : Super Duplex 2507 comply with NACE MR0175/ISO15156
Tube type : Seamless
Condition : Bright annealed
Length : Up to 10000 meters long per reel
Qualification : Hydrostatic tested
Application : Oil and gas fields
Surface : Metallic bright
Specialty : High-pressure hydraulic
Price : Negotiable
Stainless 2507 Geothermal Precision Coil Tubing Bright Annealed Stress Corrosion
A value offer for your umbilical tube challenges
The offshore industry is facing new challenges with tougher operating conditions that are significantly impacting the performance of the umbilical. Subsea umbilical systems for deep and ultra-deep offshore projects are more and more demanding regarding injection capacities, number of functionalities, power requirements and increased tie-back lengths.
Quality Assurance
| Non Destructive Tests: Hydrostatic Eddy Current Surface Roughness Dimensional Analysis
| Destructive Tests: Yield Strength Tensile Strength Elongation Positive Material Identification (PMI) Grain Size Rockwell Hardness |
MEILONG has been supplying the world’s best coiled tubes up to 3,234 lbs (1,467 kgs) and 14,764 ft (4500 mtrs) length without orbital butt welding.
Bright annealing treated, our coiled tubes are excellent in both internal and external surface quality.
Our coiled tubes are specially used in oil and gas industry requiring a higher level of reliability.
All the products are performed and delivered after ECT as well as hydrostatic & ovality test satisfying ASTM standards.
Available size and alloy materials
| Materials | Imperial Size | Metric Size | |||
| OD (in.) | WT (in.) | OD (mm) | WT (mm) | ||
| SS316L Duplex 2205 Super Duplex 2507 Incoloy 825 Inconel 625 | 1/8 | 0.125 | 0.028 | 3.18 | 0.71 |
| 1/8 | 0.125 | 0.035 | 3.18 | 0.89 | |
| 1/4 | 0.250 | 0.035 | 6.35 | 0.89 | |
| 1/4 | 0.250 | 0.049 | 6.35 | 1.24 | |
| 1/4 | 0.250 | 0.065 | 6.35 | 1.65 | |
| 3/8 | 0.375 | 0.035 | 9.53 | 0.89 | |
| 3/8 | 0.375 | 0.049 | 9.53 | 1.24 | |
| 3/8 | 0.375 | 0.065 | 9.53 | 1.65 | |
| 3/8 | 0.375 | 0.083 | 9.53 | 2.11 | |
| 1/2 | 0.500 | 0.049 | 12.70 | 1.24 | |
| 1/2 | 0.500 | 0.065 | 12.70 | 1.65 | |
| 1/2 | 0.500 | 0.083 | 12.70 | 2.11 | |
| 5/8 | 0.625 | 0.049 | 15.88 | 1.24 | |
| 5/8 | 0.265 | 0.065 | 15.88 | 1.65 | |
| 5/8 | 0.625 | 0.083 | 15.88 | 2.11 | |
| 3/4 | 0.750 | 0.049 | 19.05 | 1.24 | |
| 3/4 | 0.750 | 0.065 | 19.05 | 1.65 | |
| 3/4 | 0.750 | 0.083 | 19.05 | 2.11 | |
Super Duplex Stainless 2507, Chemical composition
| Element | Composition, % |
| Chromium | 24.0-26.0 |
| Nickel | 6.0-8.0 |
| Molybdenum | 3.0-5.0 |
| Manganese | 1.2 max. |
| Silicon | 0.8 max. |
| Carbon | 0.030 max. |
| Sulfur | 0.020 max. |
| Phosphorous | 0.035 max. |
| Nitrogen | 0.24-0.32 |
Application: Super duplex alloy combining excellent strength with good corrosion resistance in high chloride and seawater environments
Tensile strength, min.: 116ksi (800MPa)
Yield strength, min.: 80ksi (550MPa)
Elongation in 2 in., min.: 15%
Hardness, max.: Brinell 310, or Rockwell C 32
Production Process
Welded & Redrawn Tubing
Strip splice welds join lengths of cold rolled strip to enable long lengths between orbital welds (greater than 14,500 ft between orbital welds is achievable). The strip is formed into a tubular cross section and longitudinally seam welded using the gas tungsten arc (GTAW) process. The tubing is first sunk to an intermediate outside diameter, heat treated, and make the same process to obtain the desired size.
Seamless & Redrawn Tubing
Seamless extruded tube hollows are drawn or drawn / sunk to final size to produce seamless tubing coils 500 to 2,000 ft. long, depending upon the size. The tubing is heat treated and joined by orbital welding to achieve the desired length. The final material condition of the tubing is heat treated.
Super Duplex Stainless 2507 material provides excellent corrosion resistance in chloride-containing environments.
All Super Duplex Stainless 2507 control line tubing offered by MEILONG are made from a controlled-chemistry. Super Duplex Stainless 2507 material with minimum pitting resistance equivalent (PRE) value of 42.5
Size include 1/4’’, 3/8’’, 1/2’’, 5/8’’, 3/4’’, and 1 in. outside diameter.
Tubing nominal wall thickness meets ASTM A-789
Tube markings include size, material type/grade, specification, heat number, and other information.
Application
Oil and Gas: Subsea
Sub-Surface Safety Valves (SSSV) / Umbilicals: Tubes filled with Hydraulic Fluid which run from floating platform or FPSO to the well head on the sea floor.
Oil and Gas: Downhole
Downhole Control Lines: Tubes running from above ground surface controls into a downhole well to the location of the well’s safety valve.
Geothermal
Calcite Inhibition System: Carries chemicals into earth’s crust to flash point of water in a geothermal well; injected to break down calcite deposits and extend life of the well.
Instrumentation
Common connection tubing for control panels, pneumatic equipment, and fluid lines.
Norm Equivalence
| Grade | UNS No | Euro norm | Japanese | |
| No | Name | JIS | ||
| Alloy | ASTM/ASME | EN10216-5 | EN10216-5 | JIS G3463 |
| 316L | S31603 | 1.4404, 1.4435 | X2CrNiMo17-12-2 | SUS316LTB |
| 2205 | S31803 | 1.4462 | X2CrNiMoN22-5-3 | SUS329J3LTB |
| 2507 | S32750 | 1.4410 | X2CrNiMoN25-7-4 | |
| 625 | N06625 | 2.4856 | NiCr22Mo9Nb | |
| 825 | N08825 | 2.4858 | NiCr21Mo | |
Since 1999, Meilong Tube Co., Ltd. has produced long coils of stainless steel and high nickel alloy tubing for numerous oil and gas applications, including hydraulic power, monitoring and control equipment, instrumentation, injection lines, down-hole safety valve control, subsea umbilical applications. Unique manufacturing capabilities and processes allow Meilong to produce the longest continuous length control line tubing available in stainless steels and high nickel alloys.
Our coiled tubing is available in a number of high performance corrosion resistant stainless steels and high nickel alloys, including 300 series, Incoloy, Inconel, capable of withstanding a variety of severe environmental conditions.
We specialize in manufacturing small diameter tubing ranging from 0.125 inch to 1 inch outside diameter (3.18mm to 25.4 mm) and a variety of wall thickness. All tubing is level wound coiled on various size spools, and products are tested and evaluated for specific applications before delivery. Our engineering staff welcome the opportunity to work with customers to solve special problems.
Meilong’s seamless control line tubing is drawn from seamless extruded tube hollows to ensure absolute product safety and reliability. Our seamless line tubing is one continuous length of tubing, completely free of any welded joints or seams. Long length coils reduce installation time and costs by eliminating the need for excessive joints preparation and fittings. Elimination of excessive fittings increase reliability and assures a leak-free system. We are capable of 100% hydrotesting each coil.
In meeting customer’s requirements, our tubing can be encapsulated in various materials such as thermalplastics, nylon and PVDF. Coiled seamless control line tubing offers many advantages to installers of hydraulic or pneumatic lines on offshore platforms and onshore refineries. It offers unmatched safety and reliability, while at the same time reducing the frequency of costly joint connections. Close tolerance control during manufacturing assures easy insertion and connection to fittings due to tubing’s inherent ductility.
Downhole hole & umbilical tubing
Our long length seamless coils are used extensively for chemical injection and hydraulic control in subsea and onshore wells. The long length minimizes the number of orbital welds which reduces the potential for weld-related defects and failures. Additionally, our coils have an extremely clean and smooth ID surface that is ideal for hydraulic and chemical injection systems. Seamless stainless steel coils offer short hydraulic response time, greater collapse strength, and elimination of methanol permeation.
Vacuum annealing
Meilong takes special care during manufacturing to assure ID and OD cleanliness of control line tubing. Vacuum annealing insures volatility of metallic oxides and removal of any residual degreasing solvents or drawing lubricants. Vacuum annealing our stainless steel tubing insures a bright, cosmetically appealing surface as well as excellent mechanical properties.
Meilong commitment to quality excellence
From the time an order is received, sent through the production process, completed, and finally shipped, many levels of inspection occur to reinforce Meilong’s Quality Policy. The job of ensuring quality products extends as far as our machine operators. Meilong operators take ownership over material processed at their stations by measuring for dimensional accuracy and conducting a visual inspection of every piece.


|
|
Stainless 2507 Geothermal Precision Coil Tubing Bright Annealed Stress Corrosion Images |